BCC
α / δ ferrite
8 × ⅛ + 1 = 2 atoms per cell
01 / Iron–Carbon phase diagram
Choose an alloy. Follow it down the iron–carbon diagram, and connect the phases to the grains you would see under a microscope.
Both markers show the same temperature. Flat segments illustrate thermal arrests; slopes and durations are schematic.
Above: all melt (L). Crossing downward: the first solid appears.
Below: fully solid. Between liquidus and solidus: solid + melt.
Cooling γ across A₃ forms ferrite; across Acm forms cementite.
727 °C · 0.76 wt% C
γ → α + Fe₃C (pearlite)
1147 °C · 4.30 wt% C
L → γ + Fe₃C (ledeburite)
1493 °C · γ at 0.16 wt% C
L + δ → γ
α / δ = BCC ferrite · γ = FCC austenite · Fe₃C = cementite (6.67 wt% C). Steel range: up to 2.11 wt% C in this diagram convention; higher carbon: cast-iron range. Pearlite and ledeburite contain multiple phases.
Hover a phase region or a cell to spin it · drag to rotate · Spin for touch
α / δ ferrite
8 × ⅛ + 1 = 2 atoms per cell
γ austenite
8 × ⅛ + 6 × ½ = 4 atoms per cell
Fractions are by mass, evaluated at A₁. Pearlite reaches 100% at 0.76 wt% C. To its left, ferrite forms first; to its right, grain-boundary cementite forms first. Later small solubility changes are omitted.
Follow one vertical path
Predict → test → explain